Sadighzadeh, A., Mashayekhan, Sh., Nedaie, B., Ghorashi, A. H.. (1393). Study of sintering temperature on the structure of silicon carbide membrane. , 8(4), 169-173. doi: 10.1007/s40094-014-0145-5
A. Sadighzadeh; Sh. Mashayekhan; B. Nedaie; A. H. Ghorashi. "Study of sintering temperature on the structure of silicon carbide membrane". , 8, 4, 1393, 169-173. doi: 10.1007/s40094-014-0145-5
Sadighzadeh, A., Mashayekhan, Sh., Nedaie, B., Ghorashi, A. H.. (1393). 'Study of sintering temperature on the structure of silicon carbide membrane', , 8(4), pp. 169-173. doi: 10.1007/s40094-014-0145-5
Sadighzadeh, A., Mashayekhan, Sh., Nedaie, B., Ghorashi, A. H.. Study of sintering temperature on the structure of silicon carbide membrane. , 1393; 8(4): 169-173. doi: 10.1007/s40094-014-0145-5